METHOD FOR PRODUCING SINTERED BODY

Disclosed is a production method of a sintered body. The production method of a sintered body comprises a step of sintering, at a temperature within the range of from 900°C to 1200°C, a mixture of a manganese-based oxide and copper oxide wherein the ratio of the molar amount of copper to one mol of...

Full description

Saved in:
Bibliographic Details
Main Author SADAOKA, KAZUO
Format Patent
LanguageEnglish
French
German
Published 27.10.2010
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Disclosed is a production method of a sintered body. The production method of a sintered body comprises a step of sintering, at a temperature within the range of from 900°C to 1200°C, a mixture of a manganese-based oxide and copper oxide wherein the ratio of the molar amount of copper to one mol of manganese in the mixture is in the range of from 0.001 to 0.05.