GLASS FIBER REINFORCED SAN COMPOSITIONS WITH IMPROVED STIFFNESS AND TOUGHNESS

Thermoplastic moulding compositions comprising the following components: 5-95% of a copolymer A, 0-60% of a graft rubber B and 5-50% of thin glass fibers C. The copolymer A comprises 70-76% of vinylaromatic monomer(s) A1, 24-30% of vinyl cyanide monomer component(s) A2 and 0-50% of one or more unsat...

Full description

Saved in:
Bibliographic Details
Main Authors PONNUSWAMY, RAVI, SHON, KYUNG HO, NIESSNER, NORBERT
Format Patent
LanguageEnglish
French
German
Published 16.12.2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Thermoplastic moulding compositions comprising the following components: 5-95% of a copolymer A, 0-60% of a graft rubber B and 5-50% of thin glass fibers C. The copolymer A comprises 70-76% of vinylaromatic monomer(s) A1, 24-30% of vinyl cyanide monomer component(s) A2 and 0-50% of one or more unsaturated copolymerizable monomers A3. The thermoplastic moulding compositions are advantageously used for injection moulding.
Bibliography:Application Number: EP20080718104