POLYESTER POLYMERS WITH LOW ACETALDEHYDE GENERATION RATES AND HIGH VINYL ENDS CONCENTRATION

A polyester polymer comprising alkylene arylate units, said polymer having an It.V. of at least 0.72 dl/g, a vinyl ends concentration of at least 0.8 microequivalents per gram, an AA generation rate of less than 20 ppm are prepared by addition of a catalyst deactivator either late in the polycondens...

Full description

Saved in:
Bibliographic Details
Main Author JERNIGAN, Mary, Therese
Format Patent
LanguageEnglish
French
German
Published 14.10.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A polyester polymer comprising alkylene arylate units, said polymer having an It.V. of at least 0.72 dl/g, a vinyl ends concentration of at least 0.8 microequivalents per gram, an AA generation rate of less than 20 ppm are prepared by addition of a catalyst deactivator either late in the polycondensation or upon remelting of a solid polyester polymer.