PROCESS FOR REDUCING THE AVERAGE MOLECULAR WEIGHT OF CELLULOSE ETHERS

A process for reducing the average molecular weight of a cellulose ether comprises the step of contacting a cellulose ether with an acid to partially depolymerize it to a lower molecular weight in a diluent comprising at least 50 weight percent of an organic hydroxylic compound having at least one h...

Full description

Saved in:
Bibliographic Details
Main Author MALLON, CHARLES, B
Format Patent
LanguageEnglish
French
German
Published 10.08.2011
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process for reducing the average molecular weight of a cellulose ether comprises the step of contacting a cellulose ether with an acid to partially depolymerize it to a lower molecular weight in a diluent comprising at least 50 weight percent of an organic hydroxylic compound having at least one hydroxy group and at least two carbon atoms.
Bibliography:Application Number: EP20070755845