MANUFACTURING PROCESS FOR COATED POLYESTER FILM

A process in which a wound roll of biaxially oriented polyester film having a glass transition temperature (Tg (°C)) is annealed at a temperature T a (°C) above Tg where Tg < T a ‰¤ Tg + 100 (°C) for a time t after thermal equilibrium where 1 hour ‰¤ t ‰¤ 72 hours and cooled, for the purpose of i...

Full description

Saved in:
Bibliographic Details
Main Authors HODGSON, ANDREW, NATHAN, HASHIMOTO, KATSUYUKI, EVESON, ROBERT, WILLIAM, MACKERRON, DUNCAN, HENRY
Format Patent
LanguageEnglish
French
German
Published 20.05.2015
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process in which a wound roll of biaxially oriented polyester film having a glass transition temperature (Tg (°C)) is annealed at a temperature T a (°C) above Tg where Tg < T a ‰¤ Tg + 100 (°C) for a time t after thermal equilibrium where 1 hour ‰¤ t ‰¤ 72 hours and cooled, for the purpose of improving the shrinkage of said polyester film.
Bibliography:Application Number: EP20070712689