THERMOPLASTIC POLYCARBONATE COMPOSITIONS HAVING HIGH TOUGHNESS
A thermoplastic molding composition that features improved low-temperature properties and is thus suitable for application in exterior automotive parts is disclosed. The composition contains (A) 80 to 60 percent of a copolycarbonate wherein 65 to 75 mole percent of its structural units are derived f...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
09.01.2008
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A thermoplastic molding composition that features improved low-temperature properties and is thus suitable for application in exterior automotive parts is disclosed. The composition contains (A) 80 to 60 percent of a copolycarbonate wherein 65 to 75 mole percent of its structural units are derived from compounds of formula (I) wherein R , R , R and R independently of one another represents H, C1-C4-alkyl, phenyl, substituted phenyl or halogen, and wherein 25 to 35 mole percent of its structural units are derived from compounds of formula (II) where R , R , R and R independently one of the others denote H, CH3, Cl or Br and X is C1-C5-alkylene, C2-C5-alkylidene, C5-C6-cycloalkylene, C5-C10-cycloalkylidene and (B) 20 to 40 percent of a homopolycarbonate of bisphenol A having a melt flow rate, determined in accordance with ASTM D-1238 under 1.2 kg loading at 300° C. of 3 to 12 gm/10 minutes. |
---|---|
Bibliography: | Application Number: EP20030763116 |