HARD METAL SUBSTRATE BODY AND METHOD FOR PRODUCING THE SAME

The combined dopant (Al, Cr, V, Nb, Ta, Ti, Zr, Hf) content in the substrate is limited to 4 weight % at most. The cubic phase content in the substrate is less than 4 vol%. The binder metal content (Fe, Co, and/or Ni) in an edge zone of the substrate is up to 1 microns, preferably up to 0.5 microns,...

Full description

Saved in:
Bibliographic Details
Main Authors DAUB, WERNER, ROEDIGER, KLAUS, KASSEL, DIETER, DREYER, KLAUS, LENGAUER, WALTER, LOVONYAK, MARIANN, UCAKAR, VERA
Format Patent
LanguageEnglish
French
German
Published 11.04.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The combined dopant (Al, Cr, V, Nb, Ta, Ti, Zr, Hf) content in the substrate is limited to 4 weight % at most. The cubic phase content in the substrate is less than 4 vol%. The binder metal content (Fe, Co, and/or Ni) in an edge zone of the substrate is up to 1 microns, preferably up to 0.5 microns, falling to less than 0.5 times the binder content in the substrate interior An Independent claim is included for the method of manufacture
Bibliography:Application Number: EP20030740063