PROPYLENE TERPOLYMERS AND A PROCESS FOR THE PRODUCTION THEREOF

A process for producing terpolymers of propylene, comprising a) feeding into a slurry reactor a reaction mixture containing 50-85 w-% of propylene, 1-10 w-% of ethylene, 15-40 w-% of another C4-C8 alpha-olefin, a catalyst system maintaining olefin polymerization at said temperature conditions, and o...

Full description

Saved in:
Bibliographic Details
Main Authors MALM, BO, PITKAENEN, PAEIVI, MOTHA, KSHAMA, BJALAND, ANNE, BRITT, ACKERMANS, NINA, ALASTALO, KAUNO, MELLER, MIKA
Format Patent
LanguageEnglish
French
German
Published 12.04.2000
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process for producing terpolymers of propylene, comprising a) feeding into a slurry reactor a reaction mixture containing 50-85 w-% of propylene, 1-10 w-% of ethylene, 15-40 w-% of another C4-C8 alpha-olefin, a catalyst system maintaining olefin polymerization at said temperature conditions, and optionally hydrogen, b) polymerizing said reaction mixture at a temperature of lower than 70° C. a sufficient time to obtain a propylene terpolymer amounting to 50-99 w-% of the end product, c) transferring said reaction mixture into a gas phase reactor operating at a pressure of higher than 5 bars, preferably higher than 10 bars, optionally adding 0-30 w-% of ethylene, 0-10 w-% of another C4-C8 alpha-olefin, 0-40 w-% of propylene and optionally hydrogen, and d) continuing polymerization in said gas phase reactor for obtaining a propylene terpolymer amounting to 1-50 wt-% of the end product. The terpolymer has a melting temperature a less than 135° C., preferably less than 132° C., and it can be used for manufacturing films having good sealing properties.
Bibliography:Application Number: EP19980929463