Strontium master alloy composition having a reduced solidus temperature and method of manufacturing the same

Master alloy with 20-80% strontium, preferably 0.01-2.0% of aluminum and/or copper, and the balance essentially zinc plus impurities, and a method for preparing same and a method for modifying the microstructure of nonferrous alloys with said master alloy.

Saved in:
Bibliographic Details
Main Authors FRANKLIN, DANIEL B, VAIS, PHILIP G, BOONE, GARY W
Format Patent
LanguageEnglish
French
German
Published 21.01.2004
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Master alloy with 20-80% strontium, preferably 0.01-2.0% of aluminum and/or copper, and the balance essentially zinc plus impurities, and a method for preparing same and a method for modifying the microstructure of nonferrous alloys with said master alloy.