New propylene polymer contg. 0.01-1.5 pts.wt. nucleating agent (B) per 100 pts.wt. propylene homopolymer (A) with a melt flow index of 5-25g/10 minutes at 230 degrees C and 2.16 kg load (ISO 1133), and an isotacticity index of at least 98%. Also claimed is the prepn. of the polymer by combining (A)...

Full description

Saved in:
Bibliographic Details
Main Authors ZOLK, RALF, KERSTING, MEINOLF, WERNER, RAINER ALEXANDER
Format Patent
LanguageEnglish
French
German
Published 13.05.1998
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:New propylene polymer contg. 0.01-1.5 pts.wt. nucleating agent (B) per 100 pts.wt. propylene homopolymer (A) with a melt flow index of 5-25g/10 minutes at 230 degrees C and 2.16 kg load (ISO 1133), and an isotacticity index of at least 98%. Also claimed is the prepn. of the polymer by combining (A) and (B) in a mixing appts. at 200 - 250 degrees C.