Magnetic disk substrate and method of manufacturing the same

A magnetic disk substrate comprising 0.5 wt% to 1.0 wt% of Mo, 0.03 wt% to 0.5 wt% of O + 2N + 0.75C, and a balance of Ti. The alloy plate having a composition of above range is cold-rolled at a rolling ratio of 30% or more to form a magnetic disk substrate material, and the material is thermal-flat...

Full description

Saved in:
Bibliographic Details
Main Authors SUENAGA, HIROYOSHI, FUKAI, HIDEAKI, MINAKAWA, KUNINORI
Format Patent
LanguageEnglish
French
German
Published 31.08.1994
Edition5
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A magnetic disk substrate comprising 0.5 wt% to 1.0 wt% of Mo, 0.03 wt% to 0.5 wt% of O + 2N + 0.75C, and a balance of Ti. The alloy plate having a composition of above range is cold-rolled at a rolling ratio of 30% or more to form a magnetic disk substrate material, and the material is thermal-flattened under the following condition: 500 </= T </= -(150/11).t + 7850/11 1 </= t where T represents a thermal-flattening temperature ( DEG C), and t represents a thermal-flattening time (houre), thereby obtaining a magnetic disk substrate having the average grain size of 30 mu m or less.
Bibliography:Application Number: EP19900111229