CURABLE POLYESTER RESIN COMPOSITIONS SHOWING A LOW SHRINKAGE
Polyester-based mouldings which have been hardened with little shrinkage, do not stick in the mould and therefore can be released from the mould without damage are accessible via moulding compositions containing an unsaturated polyester of defined acid number and certain end groups.