Method for producing cold rolled titanium strip

A method for producing cold rolled titanium strips having good surface quality. The cold rolling of a titanium strip is carried out under the conditions represented by the following formula: X</=(48673/Y1.3283) where X is an average grain size ( mu m) of the pre-cold rolled titanium strip and Y i...

Full description

Saved in:
Bibliographic Details
Main Authors FUKUDA, MASAHITO, MATSUSHITA, TOMIHARU, TANABE, AKIYOSHI, MIZUTA, ATSUO, MORIGUCHI, YASUO, NAGAI, NOBUYUKI, YAMAGUCHI, YOSHIHIRO, TSUJI, KUNIO
Format Patent
LanguageEnglish
French
German
Published 02.12.1981
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for producing cold rolled titanium strips having good surface quality. The cold rolling of a titanium strip is carried out under the conditions represented by the following formula: X</=(48673/Y1.3283) where X is an average grain size ( mu m) of the pre-cold rolled titanium strip and Y is a diameter (mm) of the roll for the cold rolling.
Bibliography:Application Number: EP19810302265