A METHOD FOR REDUCING SHARKSKIN MELT FRACTURE DURING EXTRUSION OF ETHYLENE POLYMERS

A method for reducing sharkskin melt fracture during extrusion of a molten narrow molecular weight distribution linear ethylene polymer which comprises extruding said polymer through a die having a die gap greater than about 50 mils and wherein at least a portion of one surface of the die lip and/or...

Full description

Saved in:
Bibliographic Details
Main Authors BLAKESLEE III, THEODORE ROBERT, KURTZ, STUART JACOB, SCAROLA, LEONARD SEBASTIAN
Format Patent
LanguageEnglish
Published 03.04.1985
Edition4
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for reducing sharkskin melt fracture during extrusion of a molten narrow molecular weight distribution linear ethylene polymer which comprises extruding said polymer through a die having a die gap greater than about 50 mils and wherein at least a portion of one surface of the die lip and/or die land in contact with the molten polymer is at an angle of divergence or convergence relative to the axis of flow of the molten polymer through the die.
Bibliography:Application Number: EP19800100070