Rostfreier austenitischer Stahl geeignet für die Herstellung von Drähte

Austenitic stainless steel consists of wt.%:- max. 0.2 C; max 0.2 N; 0.3-4 Mn; 14-23 Cr; 5-17 Ni; 0.3-2 Si; max 0.1 S; 0.005-0.012 O; 0.00001-0.002 Al. max 0.0002 Mg; 0.00001-0.0005 Ca; max 0.005 Ti. Inside the steel area oxide inclusions as follows:- 40-60 SiO2; 5-50 MnO; 1-30 CaO; 0.1-20 MgO; 3-25...

Full description

Saved in:
Bibliographic Details
Main Author DESCAVES, FREDERIC
Format Patent
LanguageGerman
Published 09.11.2000
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Austenitic stainless steel consists of wt.%:- max. 0.2 C; max 0.2 N; 0.3-4 Mn; 14-23 Cr; 5-17 Ni; 0.3-2 Si; max 0.1 S; 0.005-0.012 O; 0.00001-0.002 Al. max 0.0002 Mg; 0.00001-0.0005 Ca; max 0.005 Ti. Inside the steel area oxide inclusions as follows:- 40-60 SiO2; 5-50 MnO; 1-30 CaO; 0.1-20 MgO; 3-25 Al2O3; 0.1-10 Cr2O3.
Bibliography:Application Number: DE19966006902T