ZUSAMMENSETZUNG UND VERFAHREN ZUR OBERFLÄCHENBEHANDLUNG ALUMINIUMHALTIGER METALLE

A surface of aluminiferous metal is brought into contact at 30 DEG C to 65 DEG C for 5 to 60 seconds with a surface treatment bath with a pH of 2.0 to 6.5 that contains phosphate ion, condensed phosphate ion, and a water soluble polymer in the following weight proportions: 1 - 30 : 0.1 - 10 : 0.2 -...

Full description

Saved in:
Bibliographic Details
Main Authors YOSHIDA, MASAYUKI, AOKI, TOMOYUKI
Format Patent
LanguageGerman
Published 27.04.2000
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A surface of aluminiferous metal is brought into contact at 30 DEG C to 65 DEG C for 5 to 60 seconds with a surface treatment bath with a pH of 2.0 to 6.5 that contains phosphate ion, condensed phosphate ion, and a water soluble polymer in the following weight proportions: 1 - 30 : 0.1 - 10 : 0.2 - 20. This is followed by a water rinse and drying by heating. The water soluble polymer has a chemical structure conforming with formula (I), in which (i) each of X and X represents a hydrogen atom, a C1 to C5 alkyl group, or a C1 to C5 hydroxyalkyl group; (ii) each of Y and Y represents a hydrogen atom or a moiety "Z" that conforms to formula (II) or (III), wherein each of R , R , R , R , and R represents a C1 to C10 alkyl group or a C1 to C10 hydroxyalkyl group; (iii) the average value for the number of Z moieties substituted on each phenyl ring in the polymer molecule is from 0.2 to 1.0; (iv) n is an integer with a value from 2 to 50; and (v) each polymer molecule contains at least one Z moiety.
Bibliography:Application Number: DE19956012049T