NICKEL-CHROM-MOLYBDAEN-LEGIERUNG

The use of an alloy containing 22.0 to 24.0% of chromium, 15.0 to 16.5% of molybdenum, up to 0.3% of tungsten, up to 1.5% of iron, up to 0.4% of vanadium, 0.1 to 0.4% of aluminium, 0.001 to 0.04% of magnesium and 0.001 to 0.01% of calcium, the remainder being nickel and including unavoidable accompa...

Full description

Saved in:
Bibliographic Details
Main Authors WALLIS, ERNST., 6236 ESCHBORN, DE, ROCKEL, MANFRED. DR., 6382 FRIEDRICHSDORF, DE, HEUBNER, ULRICH. DR., 5980 WERDOHL, DE, KOEHLER, MICHAEL. DR., 6370 OBERURSEL, DE
Format Patent
LanguageGerman
Published 14.09.1989
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The use of an alloy containing 22.0 to 24.0% of chromium, 15.0 to 16.5% of molybdenum, up to 0.3% of tungsten, up to 1.5% of iron, up to 0.4% of vanadium, 0.1 to 0.4% of aluminium, 0.001 to 0.04% of magnesium and 0.001 to 0.01% of calcium, the remainder being nickel and including unavoidable accompanying elements and impurities, is proposed for the production of structural components which have very good resistance to material-removing corrosion and to pitting corrosion and crevice corrosion under very severe corrosive conditions, as prevail in present-day chemical process engineering and in current environment protection technology, such as, for example, in flue gas desulphurisation plants or plants for concentrating sulphuric acid, and which should be capable of being produced economically and without problems by hot-working and cold-working.
Bibliography:Application Number: DE19883806799