Process for producing polyacrylonitrile spinning solutions having stable viscosity

A gentle manner for producing solutions, having stable viscosity, of acrylonitrile (co)polymers having solids concentrations of 20-38% by weight comprises admixing 0.01-1% by weight, based on the solution, of an amine having a pKB < 7, heating this mixture in the course of 0.5-5 hours to 50-100 D...

Full description

Saved in:
Bibliographic Details
Main Authors ENGELHARD,HELMUT,DR, KRU,PETER, NOGAJ,ALFRED,DR, REICHARDT,MANFRED,DR
Format Patent
LanguageEnglish
German
Published 28.03.1985
Edition3
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A gentle manner for producing solutions, having stable viscosity, of acrylonitrile (co)polymers having solids concentrations of 20-38% by weight comprises admixing 0.01-1% by weight, based on the solution, of an amine having a pKB < 7, heating this mixture in the course of 0.5-5 hours to 50-100 DEG C, then, if required, adding 0.25 to 2 times the equivalent amount of an amine acceptor and waiting at least 0.1-1 hour prior to processing the solution.
Bibliography:Application Number: DE19833333145