Process for the preparation of alkali-poor alpha -alumina for ceramic purposes. Technical grade aluminum hydroxide is activated and calcinated in the presence of a mineralizing mixture comprising halides and boron compounds. The process further comprises activating aluminum hydroxide at a temperatur...

Full description

Saved in:
Bibliographic Details
Main Authors TOTH, GEB. HOEMOESTREI, MARIA, MATYASI, JOZSEF.. DR, KOEKENY, BELA.. DR., KOMAROM, HU, ZSEMBERY, LASZLO.. DR, TOTH, JOZSEF., ALMASFUEZITOE-FELSOE, HU, KAPTAY, GYOERGY-METALLURGE, PENZES, IMRE-MASCH.., ALMASFUEZITOE-FELSOE, HU
Format Patent
LanguageEnglish
Published 25.07.1991
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Process for the preparation of alkali-poor alpha -alumina for ceramic purposes. Technical grade aluminum hydroxide is activated and calcinated in the presence of a mineralizing mixture comprising halides and boron compounds. The process further comprises activating aluminum hydroxide at a temperature of 500-600 degrees C., washing the activated product with alkali-free water containing calcium ions and having a conductivity not exceeding 70 mu S/cm until the alkali content expressed in Na2O becomes lower than 0.15% by weight, adding 0.4-0.7% by weight of a mineralizing mixture to the washed product, and calcinating the same at a temperature of 1200-1350 degrees C.
Bibliography:Application Number: DE19823241582