VERFAHREN ZUR HERSTELLUNG VON POLYAETHYLENTEREPHTHALATFOLIEN
A process for improving the quality of a thermoplastic, preferably a polyethylene terephthalate film. Slit rolls of polyethylene terephthalate film are exposed to an environment maintained at a temperature in the range of between about 15 DEG C. and 35 DEG C. above the temperature at which the rolls...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | German |
Published |
06.03.1975
|
Edition | 2 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A process for improving the quality of a thermoplastic, preferably a polyethylene terephthalate film. Slit rolls of polyethylene terephthalate film are exposed to an environment maintained at a temperature in the range of between about 15 DEG C. and 35 DEG C. above the temperature at which the rolls were wound for a period of at least 24 hours. This process significantly decreases the formation of surface defects that otherwise form on the surface of the film in the rolls not so treated. |
---|---|
Bibliography: | Application Number: DE19742439985 |