Pelleting chromite ore/sodium carbonate mixes - at temps avoiding formation of decahydrate to improve pellet strength

The pellets are made by mixing the prepared ore with the Na2CO3 and feeding this to a pelletiser at >36 degrees C, pref. 40-100 degrees C, and then spraying in pre-heated water or an aq. soln. of Na2CO3 at >36 degrees C, pref. >40 degrees C. The pellets formed are then dried and roasted, th...

Full description

Saved in:
Bibliographic Details
Main Authors PATRICK BRUEN,CHARLES, WALTER SMALLEY,EDMUND, BRIAN GANCY,ALAN, GENE FRICK,DOUGLAS, WAYNE LOW,WILLIAM
Format Patent
LanguageEnglish
German
Published 02.01.1976
Edition2
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The pellets are made by mixing the prepared ore with the Na2CO3 and feeding this to a pelletiser at >36 degrees C, pref. 40-100 degrees C, and then spraying in pre-heated water or an aq. soln. of Na2CO3 at >36 degrees C, pref. >40 degrees C. The pellets formed are then dried and roasted, the absence of Na2CO3 10 H2O giving the pellets adequate green strength.
Bibliography:Application Number: DE19742426915