PROCESS FOR PREPARING POLYPROPYLENE

Stereoregular polymers having a molecular weight distribution of less than 5.0 and an isotactic index in excess of 96 percent are produced by polymerizing an alpha-olefin having 3 to 8 carbon atoms in a low pressure gas phase fluid bed process at a temperature in excess of 80 DEG C employing a heat...

Full description

Saved in:
Bibliographic Details
Main Authors HAN TAI LIU, BRADY ROBERT CONVERSE, STAKEM FRANCIS GREGORY, NOSHAY ALLEN
Format Patent
LanguageEnglish
Published 11.12.1996
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Stereoregular polymers having a molecular weight distribution of less than 5.0 and an isotactic index in excess of 96 percent are produced by polymerizing an alpha-olefin having 3 to 8 carbon atoms in a low pressure gas phase fluid bed process at a temperature in excess of 80 DEG C employing a heat stable catalyst system comprising (a) a solid catalyst component containing magnesium, titanium, halide and a polycarboxylic acid ester containing two coplanar ester groups attached to adjacent carbon atoms, as inside electron donor, (b) an organoaluminum cocatalyst, and (c) a silicon compound containing a silicon-oxygen-carbon linkage, as outside electron donor.
Bibliography:Application Number: CS19880003395