Method for modification of zeolite molecular sieve outer surface acidity

The invention relates to a method for using chemical reaction deposit to decorate the outer surface acid of ZSM-5 zeolite. Wherein, said method is characterized in that the silicone grease and the molecule screen are reacted in sealed container at 140-170Deg.C to be cooled and baked; and it uses cyc...

Full description

Saved in:
Bibliographic Details
Main Author XIANGSHENG,WANG WANG
Format Patent
LanguageEnglish
Published 14.03.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a method for using chemical reaction deposit to decorate the outer surface acid of ZSM-5 zeolite. Wherein, said method is characterized in that the silicone grease and the molecule screen are reacted in sealed container at 140-170Deg.C to be cooled and baked; and it uses cyclohexane solution of ethyl orthosilicate at 1-2.0mol/l; therefore, the silicon atom of ethyl orthosilicate can be completely carried by the molecule screen; and then left slag will not contain silicone grease. The invention has high carry efficiency of silicone grease, that only carrying the micrometer ZSM-5 one time while the opposite selectivity of catalyst can reach 90%, and carrying nanometer ZSM-5 two times while the opposite selectivity of catalyst can reach 90%.
Bibliography:Application Number: CN2006147961