Process for preparing poly(trimethylene 1,3-terephthalate) fiber

The present invention relates to a process for spinning poly(trimethylene terephthalate) filaments/yarn. The poly(trimethylene terephthalate) has a number average molecular weight of at least about 26500 and a melt viscosity of at least about 350 Pascals at 250° C. and 48.65 per second shear rate. I...

Full description

Saved in:
Bibliographic Details
Main Author CHANG JING CHUNG,DOMMEL RICHARD L
Format Patent
LanguageEnglish
Published 31.01.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The present invention relates to a process for spinning poly(trimethylene terephthalate) filaments/yarn. The poly(trimethylene terephthalate) has a number average molecular weight of at least about 26500 and a melt viscosity of at least about 350 Pascals at 250° C. and 48.65 per second shear rate. It is spun and the filaments are converged into yarn. The filaments have a denier greater than 1 and the yarn has a denier greater than 210.
Bibliography:Application Number: CN200580001824