Process for the preparation of a nickel/phosphorus ligand catalyst for olefin hydrocyanation
A process for producing anhydrous nickel chloride comprising treating hydrated nickel chloride at a temperature of about 200 to about 240°C for a time less than 12 hours.
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
24.01.2007
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A process for producing anhydrous nickel chloride comprising treating hydrated nickel chloride at a temperature of about 200 to about 240°C for a time less than 12 hours. |
---|---|