Process for the preparation of a nickel/phosphorus ligand catalyst for olefin hydrocyanation

A process for producing anhydrous nickel chloride comprising treating hydrated nickel chloride at a temperature of about 200 to about 240°C for a time less than 12 hours.

Saved in:
Bibliographic Details
Main Author CHU LUIS A.,HERRON NORMAN,MOLOY KENNETH G.,CLARKSON LUCY M.,MCKINNEY RONALD J.,TEKIE ZERU
Format Patent
LanguageEnglish
Published 24.01.2007
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process for producing anhydrous nickel chloride comprising treating hydrated nickel chloride at a temperature of about 200 to about 240°C for a time less than 12 hours.
Bibliography:Application Number: CN200610105497