Process for preparing mesoporous silicon dioxide spiral coil

The invention discloses a making method of dielectric-hole silica spiral pipe, which comprises the following steps: dissolving 100g per L glucose in the water; stewing for 3-6 at 160-190 deg.c to obtain polyglucose water solution; blending polyglucose water solution, three-segmented macromolecular p...

Full description

Saved in:
Bibliographic Details
Main Author LIN,GAO DONG
Format Patent
LanguageEnglish
Published 27.12.2006
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a making method of dielectric-hole silica spiral pipe, which comprises the following steps: dissolving 100g per L glucose in the water; stewing for 3-6 at 160-190 deg.c to obtain polyglucose water solution; blending polyglucose water solution, three-segmented macromolecular polymeric surface activist (even molecular weight is 5800) of divinyl ether polyepoxide-divinyl propone polyepoxide-divinyl ether polyepoxide and 2 mol per L norbiline solution phase at 50:1:40:2 proportion; adding silicic acid ethoxy group; hydrolyze silicic acid ethoxy group completely in the sealing container; heating to 160-190 deg.c; insulating for 24 h; separating; washing; drying; sintering for 6-8 h at 550-650 deg.c; cooling to indoor temperature to obtain dielectric-hole silica spiral pipe with three-grade self-assemblage pattern.
Bibliography:Application Number: CN200610088308