Ultra low melt toners comprised of crystalline resins

A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70 DEG C and a recrystallization point of at least 47 DEG C exhibits improved document offset properties and improved heat cohesion. Annealing the toner further...

Full description

Saved in:
Bibliographic Details
Main Author SACRIPANTE GUERINO G.,ZHOU KE,HAWKINS MICHAEL S.,NOSELLA KIMBERLEY D.,ZWARTZ EDWARD G.,MIHAI NICOLETA,FARRUGIA VALERIE M.,DRAPPEL STEPHAN V.,GERROIR PAUL J
Format Patent
LanguageEnglish
Published 27.09.2006
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70 DEG C and a recrystallization point of at least 47 DEG C exhibits improved document offset properties and improved heat cohesion. Annealing the toner further improves the heat cohesion and morplzology of the toner.
Bibliography:Application Number: CN200610067368