Production of Mn-Zn ferrite from waste magnesium dioxide batteries
The invention includes hydrothermal method and sol gel method. The hydrothermal includes following steps: leaching; filter; solution composition adjustment; hydrothermal reaction; filter; wash and dry; The sol gel method includes following steps: liquid extraction; filter and insoluble matter remove...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English |
Published |
27.07.2005
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Summary: | The invention includes hydrothermal method and sol gel method. The hydrothermal includes following steps: leaching; filter; solution composition adjustment; hydrothermal reaction; filter; wash and dry; The sol gel method includes following steps: liquid extraction; filter and insoluble matter remove; solution composition adjustment; sol gel preparation; the xerogel is calcined at 600-650deg.C, or at normal temperature and pressure. |
---|---|