Prepn process of tantalum-containing carbon-base composite material precursor

The preparation process of tantalum-containing carbon-base composite material precursor includes mixing coal tar pitch or petroleum asphalt of softening point of 60-80 deg.c and tantalum chloride in the mass ratio of 100 to 1-20 in inert atmosphere and water-less environment; and reaction at 260-420...

Full description

Saved in:
Bibliographic Details
Main Authors LANG LIU, XIUTAO LI, JINGLI SHI
Format Patent
LanguageEnglish
Published 13.07.2005
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The preparation process of tantalum-containing carbon-base composite material precursor includes mixing coal tar pitch or petroleum asphalt of softening point of 60-80 deg.c and tantalum chloride in the mass ratio of 100 to 1-20 in inert atmosphere and water-less environment; and reaction at 260-420 deg.c and self pressurizing or 0.3-1.0 MPa pressure while mechanical stirring for 4-10 hr. The preparation process is simple and low in cost, and the tantalum-containing carbon-base composite material precursor may be used as the soaking agent, adhesive or self-sintering material for preparing high performance tantalum-containing carbon-base composite material.
Bibliography:Application Number: CN2004164579