Polyolefin resin/recovered paper powder/inorganic mineral composite material and preparing method thereof
The invention is a composite material with polyolefin resin, recovered paper powder and inorganic mineral powder as main raw material, the corresponding preparing ratio =1:3:2 -10:5:16. It has advantages of high intensity, good tenacity, stable construction size, and good resistance to creep. It can...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
30.06.2004
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention is a composite material with polyolefin resin, recovered paper powder and inorganic mineral powder as main raw material, the corresponding preparing ratio =1:3:2 -10:5:16. It has advantages of high intensity, good tenacity, stable construction size, and good resistance to creep. It can also use powder coal ash.
一种以聚烯烃树脂及回收纸粉.无机矿粉为主要原料的复合材料,其配比值为聚烯烃树脂∶回收纸粉∶无机矿粉=1∶3∶2~10∶5∶16。其特点是强度大、韧性好、结构尺寸稳定、抗蠕变性好,可以用回收聚烯烃树脂回收纸粉,还可以用粉煤灰等,合理、有效的利用资源。 |
---|---|