Recovery and shaping process of poly propylene, phenol formaldehyde resin, polyurethane composite waste material
A process for reclaiming the rejected composition of polypropene, phenolic resin and polyurethane, that is, the leftover of internal decoration for car, includes pulverizing, proportionally mixing it with polypropene, coupling agent and assistant, heating until the mixture is fused, putting the glas...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
17.01.2007
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A process for reclaiming the rejected composition of polypropene, phenolic resin and polyurethane, that is, the leftover of internal decoration for car, includes pulverizing, proportionally mixing it with polypropene, coupling agent and assistant, heating until the mixture is fused, putting the glass fibre cloth in mould, pouring the fused mixture, pressing, cooling and demoulding. |
---|---|