Preparation method of bridge floor crack pouring material suitable for cold environment and bridge floor crack pouring material

The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring material.The preparation method comprises the steps that 70-80 parts by mass of petroleum asphalt is heated to 165-175 DEG C in a vessel, 4-8 parts...

Full description

Saved in:
Bibliographic Details
Main Authors HUANG WEIHAN, MA YIDONG, CHEN XIANHUA, WANG ZHIBIN, CUI XU, SHI HAONAN, XU GANG, QIU WENLI, ZHUO SHANGZHI
Format Patent
LanguageChinese
English
Published 16.07.2024
Subjects
Online AccessGet full text

Cover

Loading…
Abstract The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring material.The preparation method comprises the steps that 70-80 parts by mass of petroleum asphalt is heated to 165-175 DEG C in a vessel, 4-8 parts by mass of a reinforcing agent is gradually added, and after adding is completed, a high-speed shearing machine is used for shearing for 30-40 min at the speed of 5000-6000 r/min; raising the temperature to 190-200 DEG C, sequentially adding 16-22 parts by mass of a toughening agent and 1-1.5 parts by mass of an active agent, and shearing for 1-1.5 hours by using a high-speed shearing machine at the speed of 5000r/min; the temperature is lowered to 170 DEG C to 180 DEG C, the speed of a shearing machine is adjusted to 3000 r/min to 3500 r/min, 0.03-0.06 part by mass of a stabilizer is gradually added, and development is conducted for 30 min to 60 min; quickly pouring into a storage container after development to o
AbstractList The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring material.The preparation method comprises the steps that 70-80 parts by mass of petroleum asphalt is heated to 165-175 DEG C in a vessel, 4-8 parts by mass of a reinforcing agent is gradually added, and after adding is completed, a high-speed shearing machine is used for shearing for 30-40 min at the speed of 5000-6000 r/min; raising the temperature to 190-200 DEG C, sequentially adding 16-22 parts by mass of a toughening agent and 1-1.5 parts by mass of an active agent, and shearing for 1-1.5 hours by using a high-speed shearing machine at the speed of 5000r/min; the temperature is lowered to 170 DEG C to 180 DEG C, the speed of a shearing machine is adjusted to 3000 r/min to 3500 r/min, 0.03-0.06 part by mass of a stabilizer is gradually added, and development is conducted for 30 min to 60 min; quickly pouring into a storage container after development to o
Author CUI XU
XU GANG
SHI HAONAN
WANG ZHIBIN
HUANG WEIHAN
ZHUO SHANGZHI
MA YIDONG
QIU WENLI
CHEN XIANHUA
Author_xml – fullname: HUANG WEIHAN
– fullname: MA YIDONG
– fullname: CHEN XIANHUA
– fullname: WANG ZHIBIN
– fullname: CUI XU
– fullname: SHI HAONAN
– fullname: XU GANG
– fullname: QIU WENLI
– fullname: ZHUO SHANGZHI
BookMark eNqNzD0OwjAMQOEMMPB3B3MAhqpFZUUViAkxsFdu45aIxI7clJWrAxIH6PSWT29pZixMC_O-KUVUTE4YAqWHWJAOGnW2J-i8iEKr2D4hyqiOewiYSB16GEaXsPFf9TPiLRC_nAoH4gTIdsplbeYd-oE2_67M9ny6V5cdRalpiNgSU6qra5Yd8qIoi_0xn2I-rIlLHw
ContentType Patent
DBID EVB
DatabaseName esp@cenet
DatabaseTitleList
Database_xml – sequence: 1
  dbid: EVB
  name: esp@cenet
  url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP
  sourceTypes: Open Access Repository
DeliveryMethod fulltext_linktorsrc
Discipline Medicine
Chemistry
Sciences
DocumentTitleAlternate 一种适用于寒冷环境的桥面灌缝材料的制备方法及桥面灌缝材料
ExternalDocumentID CN118344745A
GroupedDBID EVB
ID FETCH-epo_espacenet_CN118344745A3
IEDL.DBID EVB
IngestDate Fri Oct 04 04:58:32 EDT 2024
IsOpenAccess true
IsPeerReviewed false
IsScholarly false
Language Chinese
English
LinkModel DirectLink
MergedId FETCHMERGED-epo_espacenet_CN118344745A3
Notes Application Number: CN202410587282
OpenAccessLink https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240716&DB=EPODOC&CC=CN&NR=118344745A
ParticipantIDs epo_espacenet_CN118344745A
PublicationCentury 2000
PublicationDate 20240716
PublicationDateYYYYMMDD 2024-07-16
PublicationDate_xml – month: 07
  year: 2024
  text: 20240716
  day: 16
PublicationDecade 2020
PublicationYear 2024
RelatedCompanies HEBEI XIONGAN JINGDE HIGHWAY CO., LTD
RelatedCompanies_xml – name: HEBEI XIONGAN JINGDE HIGHWAY CO., LTD
Score 3.6874638
Snippet The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring...
SourceID epo
SourceType Open Access Repository
SubjectTerms CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
Title Preparation method of bridge floor crack pouring material suitable for cold environment and bridge floor crack pouring material
URI https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240716&DB=EPODOC&locale=&CC=CN&NR=118344745A
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwjV3NS8MwFH_MKepNp6LzgwjSW9Fq222HIi7tGMK6IlN2G2mT4HQ0pe0QvPivm2Sd20XxFpLwIB-_5L2X_N4DuIp5u3NLeNtMqEVMW2LCbFNOTcJiu8WYwyzthxyEbv_Zfhw74xq8LbkwOk7ohw6OKBGVSLyX-rzOVk4sX_-tLK7jqawS972R5xuVdazNE9fwu14QDf0hNjD2cGiET57Uo1VsO9t52IBNqUa3FBqCl65ipWTrV0pvD7YiKS0t96H2-dqAHbzMvNaA7UH14C2LFfaKA_iKcrYI1C1StEj8jARHC8YV4jMhcpTkJHlHmdDcQySVUb2_UDGflooihbjqI2YUrfHbEEnpf6QcwmUvGOG-KUcy-Zm2CQ5Xg747gnoqUnYMyLKokzBll0hbihOno3Q6krgdGsetG2qdQPN3Oc2_Gk9hVy2B8nxa7hnUy3zOzuWVXcYXeq6_AUtNns4
link.rule.ids 230,309,783,888,25576,76876
linkProvider European Patent Office
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwjV3NT8IwFH9BNOJNUaP4VROz26LTbbDDYqSDoMIgBg030q1tRMlKthETL_7rtgWEi8Zb0zYv6cevfe-1v_cALiJe864Jr5kxtYhpS0yYNcqpSVhkVxlzmKX9kJ3QbT3bDwNnUIC3BRdGxwn90MERJaJiifdcn9eTpRMr0H8rs8toJKvEbbPvB8bcOtbmiWsEdb_R6wZdbGDs49AIn3ypR6vYdrZztwbrUsWuKjQ0XuqKlTJZvVKa27DRk9KSfAcKn69lKOFF5rUybHbmD96yOMdetgtfvZTNAnWLBM0SPyPB0YxxhfhYiBTFKYnf0URo7iGSyqjeXyibjnJFkUJc9RFjilb4bYgk9D9S9uC82ejjlilHMvyZtiEOl4O-2YdiIhJ2AMiyqBMzZZdIW4oTx1M6HYldj0ZR9Ypah1D5XU7lr8YzKLX6nfawfR8-HsGWWg7lBbXcYyjm6ZSdyOs7j071vH8D63ChwQ
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Preparation+method+of+bridge+floor+crack+pouring+material+suitable+for+cold+environment+and+bridge+floor+crack+pouring+material&rft.inventor=HUANG+WEIHAN&rft.inventor=MA+YIDONG&rft.inventor=CHEN+XIANHUA&rft.inventor=WANG+ZHIBIN&rft.inventor=CUI+XU&rft.inventor=SHI+HAONAN&rft.inventor=XU+GANG&rft.inventor=QIU+WENLI&rft.inventor=ZHUO+SHANGZHI&rft.date=2024-07-16&rft.externalDBID=A&rft.externalDocID=CN118344745A