Preparation method of bridge floor crack pouring material suitable for cold environment and bridge floor crack pouring material

The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring material.The preparation method comprises the steps that 70-80 parts by mass of petroleum asphalt is heated to 165-175 DEG C in a vessel, 4-8 parts...

Full description

Saved in:
Bibliographic Details
Main Authors HUANG WEIHAN, MA YIDONG, CHEN XIANHUA, WANG ZHIBIN, CUI XU, SHI HAONAN, XU GANG, QIU WENLI, ZHUO SHANGZHI
Format Patent
LanguageChinese
English
Published 16.07.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a preparation method of a bridge floor crack pouring material suitable for a cold environment and the bridge floor crack pouring material.The preparation method comprises the steps that 70-80 parts by mass of petroleum asphalt is heated to 165-175 DEG C in a vessel, 4-8 parts by mass of a reinforcing agent is gradually added, and after adding is completed, a high-speed shearing machine is used for shearing for 30-40 min at the speed of 5000-6000 r/min; raising the temperature to 190-200 DEG C, sequentially adding 16-22 parts by mass of a toughening agent and 1-1.5 parts by mass of an active agent, and shearing for 1-1.5 hours by using a high-speed shearing machine at the speed of 5000r/min; the temperature is lowered to 170 DEG C to 180 DEG C, the speed of a shearing machine is adjusted to 3000 r/min to 3500 r/min, 0.03-0.06 part by mass of a stabilizer is gradually added, and development is conducted for 30 min to 60 min; quickly pouring into a storage container after development to o
Bibliography:Application Number: CN202410587282