Low-energy-consumption confidential glass and production method thereof

The invention discloses low-energy-consumption secrecy glass and a production method, and belongs to the technical field of secrecy display electronic glass, the low-energy-consumption secrecy glass comprises a secrecy glass body, the two faces of the secrecy glass body are provided with a glass A f...

Full description

Saved in:
Bibliographic Details
Main Authors YOU DANDAN, DING PINGPING, WU XUETONG, KAN LEI, LI ZHIYONG, FAN YUSHI
Format Patent
LanguageChinese
English
Published 18.06.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses low-energy-consumption secrecy glass and a production method, and belongs to the technical field of secrecy display electronic glass, the low-energy-consumption secrecy glass comprises a secrecy glass body, the two faces of the secrecy glass body are provided with a glass A face and a glass B face respectively, the width of the secrecy glass body ranges from 300 mm to 3500 mm, and the thickness of the secrecy glass body ranges from 20 mm to 30 mm. The thickness range of the confidential glass body is 50-700 [mu] m, the warping range of the confidential glass body is 0-500 [mu] m, and the non-flow thickness of the confidential glass body is 0-30 [mu] m. According to the liquid crystal display panel glass, the process procedure for producing the liquid crystal display panel glass can be effectively optimized, the complexity of the process procedure is reduced, meanwhile, the convenience during production operation is improved, waste of raw materials is avoided, and the cost during displa
Bibliography:Application Number: CN202410310902