Summary:The invention discloses a method for reducing the surface roughness of an aluminum workpiece before anodic oxidation. The method comprises the following steps: step 1, degreasing; step 2, soaking with pure water; step 3, blow-drying; step 4, abrasive paper grinding; step 5, chemical accurate grinding; step 6, soaking with pure water; step 7, blow-drying; step 8, carrying out glare flashlight inspection; step 9, roughness measurement: measuring the surface roughness of the product, and if Ra is greater than 0.2 [mu] m, returning to the step 4 until Ra is less than 0.2 [mu] m; step 10, hanging an anode; the whole complete process of degreasing, rough grinding, chemical accurate grinding, strong light inspection and roughness measurement is adopted for cleaning detection, chemical and physical modes are utilized, dry grinding and wet grinding are combined, the roughness of the product can be effectively reduced before anodic oxidation, the roughness required by anodic oxidation is 100% reached, and the product q
Bibliography:Application Number: CN202410053571