The liquid crystal polyester composition comprises the following components in parts by weight: 38-70 parts of liquid crystal polyester; 10 to 20 parts of carbon fiber; 10 to 20 parts of hollow glass beads; wherein the average retention length of the carbon fibers is 120-150 microns, the diameter ra...

Full description

Saved in:
Bibliographic Details
Main Authors ZHOU GUANGLIANG, JIANG SUJUN, LIU YAO, CHEN PINGXU, XIAO ZHONGPENG, YE NANBIAO, SONG CAIFEI
Format Patent
LanguageChinese
English
Published 05.04.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The liquid crystal polyester composition comprises the following components in parts by weight: 38-70 parts of liquid crystal polyester; 10 to 20 parts of carbon fiber; 10 to 20 parts of hollow glass beads; wherein the average retention length of the carbon fibers is 120-150 microns, the diameter ranges of the hollow glass beads are as follows: D50 is 22-28 microns, D90 is 37-43 microns, the density is 0.40-0.44 g/cm < 3 >, and the compressive strength is 7000-9000 Psi; the content of the polyarylester is 1-15% of the sum of the weight parts of the carbon fibers and the hollow glass beads; polyarylester is bisphenol A polyarylester, terephthalic acid accounts for 40-60 mol% of the dicarboxylic acid unit, and isophthalic acid accounts for 40-60 mol% of the dicarboxylic acid unit. The liquid crystal polyester composition provided by the invention has the advantages of good mechanical properties, good thin-wall formability, low anisotropy and low density, and is suitable for injection molding of sound equipment
Bibliography:Application Number: CN202311622560