Preparation method of shrinkage-free copolyester film
The invention discloses a preparation method of a shrinkage-free copolyester film, which is characterized by comprising the following steps of: synthesizing hepta-spiro phthalic acid or nine-spiro phthalic acid by adopting a spiro benzene compound, adding hepta-spiro phthalic acid or nine-spiro phth...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
02.04.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a preparation method of a shrinkage-free copolyester film, which is characterized by comprising the following steps of: synthesizing hepta-spiro phthalic acid or nine-spiro phthalic acid by adopting a spiro benzene compound, adding hepta-spiro phthalic acid or nine-spiro phthalic acid, terephthalic acid, ethylene glycol and the like into a reaction kettle, carrying out esterification reaction, adding a catalyst and a stabilizer, and carrying out polycondensation reaction to obtain the shrinkage-free copolyester film. Finally, the shrinkage-free copolyester film is prepared by adopting a two-way stretching process. By adopting the non-shrinkage copolyester film and the preparation method thereof, the defect that in the prior art, the shrinkage rate of a PET film is large due to the longitudinal tension problem can be overcome, and the prepared non-shrinkage copolyester film has the advantages of being relatively simple to synthesize, high in mechanical strength, completely free of shrin |
---|---|
Bibliography: | Application Number: CN202311661919 |