Alkali-free glass
The present invention relates to an alkali-free glass containing, in mol% on the basis of oxides, 63% to 69% of SiO2, 8% to 13% of Al2O3, 0.5% to 4% of B2O3, 8% to 15% of MgO, 4% to 12% of CaO, 0 to 4.5% of SrO, and 0 to 1% of BaO, with [MgO]/[CaO] being 0.67 to 3.75, the value of formula (A) being...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
22.03.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The present invention relates to an alkali-free glass containing, in mol% on the basis of oxides, 63% to 69% of SiO2, 8% to 13% of Al2O3, 0.5% to 4% of B2O3, 8% to 15% of MgO, 4% to 12% of CaO, 0 to 4.5% of SrO, and 0 to 1% of BaO, with [MgO]/[CaO] being 0.67 to 3.75, the value of formula (A) being 84 or more, the value of formula (B) being 715 or less, the value of formula (C) being 200 or less, and the value of formula (D) being 15 or less.
本发明涉及一种无碱玻璃,其中,以氧化物基准的摩尔%计,所述无碱玻璃包含63%~69%的SiO2、8%~13%的Al2O3、0.5%~4%的B2O3、8%~15%的MgO、4%~12%的CaO、0~4.5%的SrO、和0~1%的BaO,并且[MgO]/[CaO]为0.67~3.75,式(A)的值为84以上,式(B)的值为715以下,式(C)的值为200以下,式(D)的值为15以下。 |
---|---|
Bibliography: | Application Number: CN202311595930 |