Preparation method of heat-conducting foam carbon and prepared heat-conducting foam carbon

The invention relates to a preparation method of heat-conducting foam carbon and the prepared heat-conducting foam carbon, and the preparation method comprises the following steps: (1) crushing an asphalt component, carrying out dry mixing on the crushed asphalt component, porous graphite and an opt...

Full description

Saved in:
Bibliographic Details
Main Authors DUAN CHUNTING, LIU JUNQING, SHENG YING, WANG HONGFEI, RUAN RUYU, ZHENG DONGFANG
Format Patent
LanguageChinese
English
Published 02.02.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a preparation method of heat-conducting foam carbon and the prepared heat-conducting foam carbon, and the preparation method comprises the following steps: (1) crushing an asphalt component, carrying out dry mixing on the crushed asphalt component, porous graphite and an optional heat-conducting reinforcing material for uniform mixing, and then carrying out compression molding; (2) treating the preformed material obtained in the step (1) for more than 10 minutes at 450-700 DEG C under normal pressure to obtain a formed material; (3) performing high-temperature treatment on the molded material obtained in the step (2) at normal pressure and in a protective atmosphere at the temperature of 900 DEG C or above to obtain a foam carbon material; a normal-pressure preparation process is adopted, the process is simple and convenient, the cost is low, a low-density porous structure and multi-stage pore size distribution are achieved through effective lap joint between porous graphite, and a la
Bibliography:Application Number: CN202210879218