Method for recovering uranium from high-quality monazite slag
The invention provides a method for recycling uranium from high-quality monazite molten slag, and belongs to the technical field of hydrometallurgy. The method comprises the following steps: 1, leaching; 2, carrying out solid-liquid separation; 3, extracting to remove iron; and 4, extracting uranium...
Saved in:
Main Authors | , , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
11.08.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a method for recycling uranium from high-quality monazite molten slag, and belongs to the technical field of hydrometallurgy. The method comprises the following steps: 1, leaching; 2, carrying out solid-liquid separation; 3, extracting to remove iron; and 4, extracting uranium. According to the method, the problem that solid-liquid separation of ore pulp is difficult is solved by adding polyacrylamide, the leaching rate of uranium, thorium and rare earth is high by adopting a high hydrochloric acid system, iron is removed and uranium is extracted step by step by utilizing a single extraction technology, the process is simple and easy to use, the uranium-iron-thorium separation effect is good, sodium diuranate prepared from uranium qualified liquid is few in impurity, high in quality and suitable for industrial application.
本发明提供了一种从独居石优溶渣中回收铀的方法,属于湿法冶金技术领域。本发明的方法包括以下步骤:1.溶浸;2.固液分离;3.萃取除铁;4.萃取提铀。本发明方法通过添加聚丙烯酰胺解决矿浆固液分离困难问题,采用高盐酸体系,铀、钍、稀土浸出率高,利用单一萃取技术分步萃取除铁提铀,工艺简单易用,铀铁钍分离效果好,铀合格液制备重铀酸钠,杂质少 |
---|---|
Bibliography: | Application Number: CN202310262348 |