Chromium ore smelting redution process

In this invention, the smelting reduction operation can be carried out in a high efficiency by charging a carbonaceous material in such an amount that total surface area is not less than 60 m per 1 ton of slag weight. Furthermore, carbon substance finely particulating through thermal crumbling under...

Full description

Saved in:
Bibliographic Details
Main Authors AIDA KIMIHARU, TAKEUCHI SHUJI, BESSHO NAGAYASU
Format Patent
LanguageEnglish
Published 19.11.1997
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:In this invention, the smelting reduction operation can be carried out in a high efficiency by charging a carbonaceous material in such an amount that total surface area is not less than 60 m per 1 ton of slag weight. Furthermore, carbon substance finely particulating through thermal crumbling under a high-temperature atmosphere inside the vessel is used as the carbonaceous material, whereby it is possible to stably conduct the smelting reduction while controlling the scattering of the carbonaceous material, and also the erosion, particularly locally erosion of refractory in the smelting reduction furnace, which was a serious problem in the conventional technique, can considerably be decreased to largely prolong the service life of refractory.
Bibliography:Application Number: CN19961091143