Preparation method of catalytic cracking catalyst with low coke yield and high BTX yield

The invention relates to a preparation method of a low-green-coke catalytic cracking catalyst without ammonia nitrogen pollution. The method comprises the following steps: mixing an unmodified NaY molecular sieve with an aluminum oxide binder, a silicon oxide binder, clay and water, pulping, perform...

Full description

Saved in:
Bibliographic Details
Main Authors ZHOU LINGPING, YUAN SHUAI, ZHANG WEILIN, ZHANG JIEXIAO, SHA HAO, SONG HAITAO, YAN JIASONG, XU MINGDE
Format Patent
LanguageChinese
English
Published 07.04.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a preparation method of a low-green-coke catalytic cracking catalyst without ammonia nitrogen pollution. The method comprises the following steps: mixing an unmodified NaY molecular sieve with an aluminum oxide binder, a silicon oxide binder, clay and water, pulping, performing spray drying, and roasting to obtain catalyst microspheres; and then, carrying out ion exchange modification, mild hydrothermal ultra-stable modification, SiCl4 gas phase ultra-stable modification, pore channel cleaning modification and gallium and/or boron active element modification treatment. The preparation method is a preparation method of the ammonia-nitrogen-pollution-free high-yield BTX catalytic cracking catalyst, the catalytic cracking catalyst which is larger in pore volume and specific surface area and better in strength can be prepared through the method, ammonia-nitrogen pollution does not exist in the whole preparation process of the catalyst, and the catalyst is environmentally friendly. And the