Low-density pouring sealant and preparation method thereof

The invention provides a preparation method of a low-density pouring sealant, which comprises the following steps: a) dehydrating trifunctional polyether and bifunctional polyether, cooling to 70-80 DEG C, adding isocyanate to react for 1-2 hours under the protection of nitrogen and stirring conditi...

Full description

Saved in:
Bibliographic Details
Main Authors DU SHUAIPENG, ZHANG YONG, LU YUCHONG, WANG JIANBIN, GUO ZHENG, MA YUMIN, SUN XIAOKANG, LI YAO, TAO XINLIANG, WANG KE, HONG CONGZHE, CAI YAOWU, FAN RUOBIN
Format Patent
LanguageChinese
English
Published 10.03.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention provides a preparation method of a low-density pouring sealant, which comprises the following steps: a) dehydrating trifunctional polyether and bifunctional polyether, cooling to 70-80 DEG C, adding isocyanate to react for 1-2 hours under the protection of nitrogen and stirring conditions, adding a catalyst to continue to react for 1-2 hours, then adding micromolecules containing hydroxyl and vinyl, continuing to react for 2-3 hours, cooling to 70-80 DEG C, adding a catalyst to react for 1-2 hours under the protection of nitrogen and stirring conditions, and cooling to 70-80 DEG C; a vinyl terminated polyurethane prepolymer is obtained; b) uniformly mixing the vinyl-terminated polyurethane prepolymer obtained in the step a) with calcium carbonate, glass beads and a vinyl silane coupling agent to obtain a component A; uniformly mixing hydrogen-containing silicone oil and a platinum catalyst to obtain a component B; the component A and the component B are mixed according to the mass ratio of 100:
Bibliography:Application Number: CN202211666158