Method for improving retention rate of carbon nanofibers in carbon paper

The invention discloses a method for improving the retention rate of carbon nanofibers in carbon paper, which comprises the following steps: adding 0.1-0.5 g by mass of carbon nanofibers into 15-25 ml by mass of ethanol, then carrying out ultrasonic treatment for 30-50 minutes, then applying the sol...

Full description

Saved in:
Bibliographic Details
Main Authors GUO DALIANG, SHA ZHOU, ZENG SHIYI, ZHANG SHENCHONG, SHEN CONGHAO, LI JING, ZHAO HUIFANG
Format Patent
LanguageChinese
English
Published 30.12.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a method for improving the retention rate of carbon nanofibers in carbon paper, which comprises the following steps: adding 0.1-0.5 g by mass of carbon nanofibers into 15-25 ml by mass of ethanol, then carrying out ultrasonic treatment for 30-50 minutes, then applying the solution subjected to ultrasonic treatment to a spray coating machine to carry out spray coating on the carbon paper, putting the coated carbon paper into a flat plate fluidized bed, and carrying out heat preservation for 30-50 minutes, thereby obtaining the retention rate of the carbon nanofibers in the carbon paper. The temperature of an upper plate is set to be 110-130 DEG C, the temperature of a lower plate is set to be 110-130 DEG C, the pressure is set to be 5-7 MPa, and the carbon paper is pressed for 15-25 min through a flat plate fluidized bed, so that the carbon paper filled with the coated carbon nanofibers is obtained. According to the invention, the retention rate of the carbon nanofibers as a filling age
Bibliography:Application Number: CN202211323115