Method for preparing carbon nanofiber with surface micropore morphology by using alkali lignin and polyacrylonitrile

The invention discloses a method for preparing carbon nanofibers with surface micropore morphology from alkali lignin and polyacrylonitrile, which comprises the following steps: sucking a polyacrylonitrile solution by using a No.1 injector, introducing the polyacrylonitrile solution into a needle op...

Full description

Saved in:
Bibliographic Details
Main Authors GUO DALIANG, LIU XIAOGANG, SHA ZHOU, SHEN CONGHAO, ZHANG SHENCHONG, LI JING, ZHAO HUIFANG
Format Patent
LanguageChinese
English
Published 30.12.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a method for preparing carbon nanofibers with surface micropore morphology from alkali lignin and polyacrylonitrile, which comprises the following steps: sucking a polyacrylonitrile solution by using a No.1 injector, introducing the polyacrylonitrile solution into a needle opening A of a No.1 electrostatic spinning machine, and using an injection pump of the No.1 electrostatic spinning machine; the alkali lignin solution is sucked by a second injector and connected into a needle opening B of a second electrostatic spinning machine, and an injection pump of the second electrostatic spinning machine is used; sticking release paper on a receiver of an electrostatic spinning machine, and spinning by using the electrostatic spinning machine; after spinning is finished, obtained precursor fibers are dried, the dried precursor fibers are put into a muffle furnace to be oxidized, and oxidized fibers are obtained; and placing the oxidized fiber in a tubular furnace, carbonizing under the protec
Bibliography:Application Number: CN202211326002