Method for producing processed body having water-repellent surface, and processed body having water-repellent surface

The invention provides a method for manufacturing a processed body having a water-repellent surface and a processed body having a water-repellent surface. The method for manufacturing a processed body having a water-repellent surface includes a step (a) in which a member comprising a crystalline or...

Full description

Saved in:
Bibliographic Details
Main Authors VAMOS, CHRISTIAN, NAKAI, YUKAKO, MARASFOY BART, RAZ ILAN, MIMURA YUTAKA
Format Patent
LanguageChinese
English
Published 11.11.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention provides a method for manufacturing a processed body having a water-repellent surface and a processed body having a water-repellent surface. The method for manufacturing a processed body having a water-repellent surface includes a step (a) in which a member comprising a crystalline or semi-crystalline polymer is brought into contact with a solvent in a solvent contact region, and a step (b) in which the member that has been brought into contact with the solvent is removed from the solvent contact region and dried. The difference in Hildbland solubility parameters between the polymer and the solvent is less than 7.5 MPa1/2, the boiling point of the solvent is higher than the crystallization temperature (Tc) of the polymer, the temperature of the solvent when the member is brought into contact with the solvent is Tc +/-50 DEG C of the polymer and is equal to or lower than the boiling point of the solvent, and the temperature of the solvent when the member is brought into contact with the solvent i
Bibliography:Application Number: CN202180024279