Deformed CoCrNiAlTi medium-entropy alloy with excellent performance in medium-high temperature interval and preparation method of deformed CoCrNiAlTi medium-entropy alloy

The invention discloses a deformed CoCrNiAlTi medium-entropy alloy with excellent performance in a medium-high temperature interval and a preparation method thereof.The alloy is prepared from, by atomic percent, 31%-35% of Co, 28%-33% of Cr, 24%-28% of Ni, 4%-7% of Al and 4%-7% of Ti, the deformed C...

Full description

Saved in:
Bibliographic Details
Main Authors DU XINGHAO, ZU RUNFENG, YANG MINGCHENG, YUAN SHUAI, SHI CHUANXIN, WANG DAPENG, WU BAOLIN, YAN FEI, KIM SUNG-YEON
Format Patent
LanguageChinese
English
Published 27.09.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a deformed CoCrNiAlTi medium-entropy alloy with excellent performance in a medium-high temperature interval and a preparation method thereof.The alloy is prepared from, by atomic percent, 31%-35% of Co, 28%-33% of Cr, 24%-28% of Ni, 4%-7% of Al and 4%-7% of Ti, the deformed CoCrNiAlTi medium-entropy alloy with the excellent performance in the medium-high temperature interval obtains high comprehensive mechanical performance in the medium-high temperature interval, and the performance of the medium-high temperature interval is improved. And the common weakness of medium-temperature brittleness of the high-temperature alloy is overcome. 本发明公开了一种中高温度区间性能优异的变形CoCrNiAlTi中熵合金及其制备方法,其中,所述合金按照原子百分比,包括如下成分:Co:31-35%、Cr:28-33%、Ni:24-28%、Al:4-7%、Ti:4-7%,所述中高温度区间性能优异的变形CoCrNiAlTi中熵合金在中高温度区间获得较高的综合力学性能,克服了高温合金普遍存在的中温脆性的弱点。
Bibliography:Application Number: CN202210756480