Method for obtaining high-orientation GOSS texture Fe-3% Si material
The invention discloses a high-orientation GOSS texture Fe-3% Si material and a preparation method thereof. The production method mainly comprises the steps of steelmaking, slab continuous casting, hot continuous rolling, normalizing, acid pickling, cold rolling, decarburization nitriding annealing,...
Saved in:
Main Authors | , , , , , , , , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
21.06.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a high-orientation GOSS texture Fe-3% Si material and a preparation method thereof. The production method mainly comprises the steps of steelmaking, slab continuous casting, hot continuous rolling, normalizing, acid pickling, cold rolling, decarburization nitriding annealing, magnesium oxide separant coating, high-temperature cover annealing and flat stretching annealing. According to the method, the Goss texture orientation degree of the finished product is remarkably improved mainly through the principle that the key process is matched with the plate texture. A large number of {100} surface textures are reserved by reserving casting blank columnar crystals, and the Goss texture with the accurate orientation is obtained on the secondary surface layer of a rolled plate under the action of shearing force in the hot rolling procedure. Decarburization nitriding annealing is conducted, and the annealing temperature and nitriding amount are matched so that the post-annealing {111} lt can be |
---|---|
Bibliography: | Application Number: CN202210246046 |