Summary:The invention provides a copper-aluminum pre-alloy, a preparation method and a diamond tool. The copper-aluminum pre-alloy comprises the following components: 12-24 parts by mass of aluminum; 4 to 6 parts by mass of zinc; 0 to 12 parts by mass of tin; 3 to 5 parts by mass of iron; 1-4 parts by mass of silicon; 3 to 5 parts by mass of nickel; and 44 to 77 parts by mass of copper. The copper-aluminum pre-alloy provided by the invention can be used for a diamond tool, the performance of the tool is improved, and the service life is prolonged. 本发明提供了一种铜铝预合金、制备方法、金刚石工具;铜铝预合金包括以下成分:铝,12质量份至24质量份;锌,4质量份至6质量份;锡,0质量份至12质量份;铁,3质量份至5质量份;硅,1质量份至4质量份;镍,3质量份至5质量份;铜,44质量份至77质量份。本发明提供的铜铝预合金可以用于金刚石工具,提高工具的性能和使用寿命。